Type IV/A (V) 42,5 R-SR - Tipo IV/A (V) 42,5 R-SR - Buzzi Unicem Italia
Type IV/A (V) 42,5 R-SR
This cement contains: 65-89% clinker with a low calcium aluminate content, 11-35% fly ash. A maximum of 5% minor constituents is permitted. The percentages indicated do not include additions of calcium sulfate and additives.
Known for its rapid early strength development and due to the low aluminate content in the clinker, this cement offers special advantages such as the high/very high resistance to sulfates, suitability for use in marine environments, and controlled development of the heat of hydration. The cement conforms to the harmonized European standard EN 197/1 and displays the CE marking as required by European regulation 305/2011 (CPR).
"SR" means that the cement is sulfate-resistant, an additional property of the product in accordance with the composition and performance requirements specified in tables 2 and 5 of EN 197/1.
CGreen
Product with a lower environmental impact formulated to uphold the principles of sustainability and offer construction solutions that meet the latest environmental standards. The criteria used to define the CGreen line are based on the GWP (Global Warming Potential) indicator, which is included in the Environmental Product Declaration (EPD) to quantify the Carbon Footprint of cement and the entire supply and production chain.
The percentage of recycled content has also been identified for each cement to define the circularity indicator by cement type.
Chemical properties
Parameter | Test method | Indicative values (1) | Specified characteristic limits |
---|---|---|---|
Sulfates (SO3) | EN 196/2 | <3,7% | <=4,0% |
Chlorides (Cl - ) | EN 196/2 | <0,08% | <=0,10% |
Pozzolanic activity test (8 days) | EN 196/5 | positive | positive |
Water-soluble chromium VI | EN 196/10 | <=2 ppm | <=2 ppm |
Physical/mechanical properties
Parameter | Test method | Indicative values (1) | Specified characteristic limits |
---|---|---|---|
Blaine specific surface | EN 196/6 | 4000-5500 cm2/g | |
Initial setting time | EN 196/3 | >100 min | >=60 min |
Volume stability | EN 196/3 | <=10 mm | <=10 mm |
ompressive strength after curing for | EN 196/1 | ||
2 days | >24,0 MPa | >=20,0 MPa | |
28 days | >48,0 MPa | >=42,5 MPa |
(1) The values represent the level above (or below) the reasonably expected median values for the parameters indicated of BUZZI UNICEM cements belonging to the type and class named in the headers. These values are calculated on a yearly basis and take into account internal self-inspection data.
Current applications
- Reinforced concrete for in-ground and above-ground works requiring good early and final strengths
- Concrete for foundations and any works in aggressive environments
- Wet-process sprayed concrete for lining tunnels
- Concrete in contact with seawater
- Sewage works
- Concrete for road and rail works
Documents